Table 2 Springiness, cohesiveness and cutting strength of extruded ISP with different biji contents
Biji (%) | Barrel temperature (°C) | Moisture content (%) | Texture |
Springiness (%) | Cohesiveness (%) | Cutting strength (N/m2) |
0 | 140 | 35 | 76.87±1.21f | 65.64±0.68h | 6.19E+04p |
45 | 81.24± 1.49c | 67.58±0.92e.f.g | 5.93E+04o |
150 | 35 | 76.47±1.17e | 66.21±1.27e.f.g.h | 6.37E+04n |
45 | 81.96±1.36c | 68.72±0.67.a.b.c.d | 5.99E+04m |
20 | 140 | 35 | 75.49± 0.43e | 64.40±1.75g.h | 5.38E+04l |
45 | 80.60±0.76b | 67.18±0.98b.c.d.e.f | 5.31E+04k |
150 | 35 | 75.74±0.67d.e | 65.75±0.66e.f.g | 5.76E+04j |
45 | 80.94± 0.72b | 68.72±0.56a.b.c | 5.32E+04i |
| 140 | 35 | 74.05±0.83c.d.e | 63.77±0.28f.g.h | 5.11E+04h |
| 45 | 79.33±0.72a.b | 65.90±0.91a.b.c.d | 4.97E+04g |
40 |
|
| 150 | 35 | 74.78±0.64c.d.e | 65.25±0.57c.d.e.f | 5.27E+04f |
| 45 | 79.12±0.81a.b | 67.52±0.93a | 4.93E+04e |
60 | 140 | 35 | 72.19±0.21c | 63.51± 0.87d.e.f | 5.01E+04d |
45 | 76.99±1.13a | 65.36±0.83a.b | 4.88E+04c |
150 | 35 | 74.48±1.07c.d | 64.66±1.37b.c.d.e | 4.95E+04b |
45 | 76.84±2.17a | 67.28±0.90a | 4.76E+04a |
Means ±SD
Values with different letters in column are significantly different (p<0.05) by Duncan’s multiple range test.